The general composition of acid-resistant refractory castables is as follows: 60%-70% acid-resistant refractory aggregate, 30%-40% powder, and 13%-16% water glass solution with a density of 1.38-1.42 g/cm3. When sodium fluorosilicate is used as a hardening accelerator, its addition amount is Read More …